BOSTON--(BUSINESS WIRE)--At the 2014 MRS Fall Meeting and Exhibit, Bruker (NASDAQ: BRKR) today introduced the NanoForce Nanoindenting and Nanomechanical Testing System to enable new discoveries in nanoscience. Nanomaterials are now found not only in research but increasingly in the product design cycle, and are playing a prominent role in industry. Determining their suitability for use in specific applications requires robust analysis of their unique capabilities. The new NanoForce system supports complete investigations of nanomechanical properties, enabling both academic research and product development to go beyond nanoindentation into full-scale studies of nanoscale material behavior on a wide range of specimen geometries, including thin films, nanostructures, MEMS and various device components.